Nickel Alloy CM 247 LC
General Technical Characteristics
Material Type: Cast heat-resistant nickel-base superalloy for directional solidification.
Grade: CM 247 LC.
Designation: CM 247 LC, Cannon-Muskegon 247 LC.
Standards / Specifications: AMS 5409, aerospace and power generation turbine industry specifications.
Alloy Base: Nickel (Ni).
Alloying System: Ni-W-Co-Cr-Al-Ta-Hf-Ti-Mo.
Primary Manufacturing Method: Vacuum Induction Melting (VIM) followed by precision vacuum investment casting with directional solidification.
Strengthening Mechanism: Precipitation hardening (approx. 62–65% $\gamma’$-phase) and solid-solution strengthening.
Key Properties: Ultra-high creep-rupture strength, exceptional creep and thermal fatigue resistance, superior DS castability.
Supply Forms: Cast remelt ingots (master alloy), directionally solidified castings, and blanks.
Chemical Composition
| Element | Content, % | Element | Content, % |
| Nickel (Ni) | Balance | Tantalum (Ta) | 3.00 – 3.40 |
| Tungsten (W) | 9.20 – 9.80 | Hafnium (Hf) | 1.20 – 1.60 |
| Cobalt (Co) | 9.00 – 9.50 | Titanium (Ti) | 0.60 – 0.90 |
| Chromium (Cr) | 7.80 – 8.40 | Molybdenum (Mo) | 0.40 – 0.60 |
| Aluminum (Al) | 5.40 – 5.80 | Carbon (C) | 0.06 – 0.08 |
| Boron (B) | 0.012 – 0.020 | Zirconium (Zr) | 0.007 – 0.020 |
| Iron (Fe) | max 0.20 | Manganese (Mn) / Silicon (Si) | max 0.05 / max 0.05 |
Mechanical and Performance Properties
ultra-high stress-rupture strength and creep resistance along the longitudinal crystal growth direction;
complete suppression of longitudinal hot tearing during directional solidification;
high ductility and impact toughness across a broad operating temperature range;
enhanced resistance to thermal fatigue and thermal shock;
excellent microstructural stability without brittle phase precipitation during prolonged service;
high compatibility with advanced thermal barrier coatings (TBC) and aluminide protective coatings.
Density: approx. 8.54 g/cm³.
Melting Range: approx. 1280 – 1365 °C.
Applications
high-pressure and intermediate-pressure turbine rotor blades for aircraft gas turbine engines;
nozzle guide vanes and stator assemblies with complex internal air-cooling channels;
high-temperature blades for next-generation stationary industrial gas turbine units;
hot-section flowpath components for jet and turboshaft engines;
thin-walled shaped castings with intricate aerodynamic geometries.
Key Features of CM 247 LC
optimized balance of refractory elements (W, Ta, Mo) and $\gamma’$-forming components (Al, Ti);
hafnium alloying (~1.4%), strengthening columnar grain boundaries and enhancing transverse ductility;
high quality repeatability when casting large and thin-walled hollow blades;
significant increase in turbine operating temperature capability and overall thermal efficiency;
minimal susceptibility to casting defects and microporosity.