  • Characteristics
  • Description

P295GH steel delivery forms

Boiler steel grades

Steel grades
EN 10028

Steel grade DIN

Dimensions mm

Special thicknesses

Thickness

Width

Length up to

P 295 GH

1.0481

5 – 120

1000 – 3500

13,000

13,14,18,26,28

Boiler sheet steel P295GH

According to its characteristics, boiler steel grade P295GH corresponds to European standards EN10028-2. Unalloyed and alloyed materials are supplied in the form of flat products designed to work under high pressure, at elevated temperatures.

The properties of steel are determined by the content of silicon, copper, nickel and molybdenum in it. At the same time, their total share should not exceed 70%.

Special properties

the ability to work at elevated temperatures, the level of which can reach 450 degrees.

Normalization of the structure occurs at a temperature of 890-950 degrees. Forging is performed within the range from 1260 to 750 degrees.

The material has no restrictions on weldability. It is possible to use manual arc, automatic arc, performed under a flux and in a protective gas environment, and electroslag welding.

Applications

EN10028-2 is used in the manufacture of various tanks, heat exchangers, boilers. At the same time, the affordable price for the boiler pipe, as well as for other elements made of this steel, ensures its considerable popularity.

The chemical composition of P295GH steel

EN 10028-2

C

0.08-0.20

Si

<0,40

Mn

0.7-1 ,5

P

<0.025

S

<0.01

Cr

<0,3

Mo

<0.08

Ni

<0,3

V

<0.02

Nb

<0,02

Ti

<0.03

Al

>0.02

Cu

<0,3

N

<0.012

Fe

Other

Mechanical properties of steel P295GH

Per EN 10028-2

+N

Nominal thickness, (mm)

< 16

16 – 40

40 – 60

60 – 100

100 – 150

150 – 250

Minimum yield strength, ReH (MPa)

295

290

285

260

235

220

Tensile strength (tensile strength) , Rm (MPa)

460-580

460-580

460-580

460-580

440-570

430-570

Minimum elongation after break, A (%)

21

Minimum absorbed energy at 20°C, J (J )

40

Minimum absorbed energy at 0°C 32°F], J (J)

34

Minimum absorbed energy at -20°C, J (J)

27

Yield strength at 50°C, ReH (MPa)

285

280

276

251

227

213

Yield strength at 100°C, ReH (MPa)

268

264

259

237

214

200

Yield strength at 150°C, ReH (MPa)

249

244

240

219

198

185

Yield strength at 200°C, ReH (MPa)

228

225

221

201

182

170

Yield strength at 250°C, ReH (MPa)

209

206

202

184

167

156

Yield strength at 300°C, ReH (MPa)

192

189

186

170

153

144

Yield strength at 350°C, ReH (MPa)

178

175

172

157

142

133

Yield strength at 400°C, ReH (MPa)

167