Nickel Alloy Rene N6
General Technical Characteristics
Material Type: Third-generation single-crystal (SX) heat-resistant nickel-base superalloy.
Grade: Rene N6 (René N6).
Designation: Rene N6, René N6, GE B50TF293.
Standards / Specifications: Aerospace and power generation turbomachinery industry specifications (General Electric B50TF293, AMS, etc.).
Alloy Base: Nickel (Ni).
Alloying System: Ni-Co-Ta-Cr-Al-W-Re-Mo-Hf-Y.
Primary Manufacturing Method: Vacuum Induction Melting (VIM) followed by precision vacuum single-crystal investment casting.
Strengthening Mechanism: Precipitation hardening (approx. 70% $\gamma’$-phase) and solid-solution strengthening with rhenium, tungsten, and tantalum.
Key Properties: Ultra-high creep-rupture strength (up to 1150 °C), complete elimination of grain boundaries, and maximum creep and thermal fatigue resistance.
Supply Forms: Ultra-high-purity cast remelt ingots (master alloy), single-crystal castings, and blanks.
Chemical Composition
| Element | Content, % | Element | Content, % |
| Nickel (Ni) | Balance | Tungsten (W) | 5.70 – 6.30 |
| Cobalt (Co) | 12.00 – 13.00 | Rhenium (Re) | 5.10 – 5.70 |
| Tantalum (Ta) | 7.00 – 7.50 | Molybdenum (Mo) | 1.20 – 1.60 |
| Chromium (Cr) | 4.00 – 4.50 | Hafnium (Hf) | 0.12 – 0.20 |
| Aluminum (Al) | 5.60 – 6.00 | Carbon (C) | 0.04 – 0.06 |
| Boron (B) | 0.003 – 0.006 | Yttrium (Y) | 0.005 – 0.020 (micro-addition) |
| Titanium (Ti) | max 0.05 | Iron (Fe) / Silicon (Si) | max 0.20 / max 0.05 |
Mechanical and Performance Properties
maximum stress-rupture strength and creep resistance among production aerospace alloys due to elevated rhenium content (~5.4%);
outstanding resistance to thermal fatigue and thermal shock owing to the low elastic modulus of the single crystal in the
<001>orientation;exceptional resistance to cyclic oxidation and protective alumina ($\text{Al}_2\text{O}_3$) scale spallation via yttrium micro-alloying;
balanced microstructural stability without brittle topologically close-packed (TCP) phase formation under operating regimes;
full compatibility with advanced platinum-aluminide (PtAl) and multi-layer thermal barrier coatings (TBC).
Density: approx. 8.97 g/cm³.
Melting Range: approx. 1330 – 1400 °C.
<001> crystallographic orientation accuracy and multi-stage vacuum heat treatment regimes, and are therefore governed by the documentation for a specific batch.Applications
single-crystal high-pressure turbine (HPT) rotor blades for modern high-thrust aircraft engines (GE90-115B, GEnx, GP7200, F119/F135 families, etc.);
cooled first-stage turbine nozzle guide vanes and stator assemblies featuring intricate internal cooling passages and film-cooling perforations;
high-temperature blades for heavy-duty stationary industrial gas turbine units of the latest classes;
hot-section flowpath components for next-generation marine and aeroderivative gas turbine engines;
critically loaded elements in rocket and aerospace turbopump assemblies.
Key Features of Rene N6
rhenium alloying (~5.4%), radically retarding diffusion-controlled creep up to 1150 °C;
yttrium (Y) micro-alloying combined with high aluminum (~5.8%), ensuring robust retention of the protective oxide scale and thermal barrier coatings;
near-zero titanium content (less than 0.05%), enhancing protective coating durability under cyclic thermal exposures;
substantial increase in turbine inlet gas temperature, improving engine fuel efficiency and thrust;
ultra-high master alloy ingot purity, minimizing the risk of single-crystal grain defects during solidification.