Nickel Alloy CMSX-4 / CMSX-4 Plus (SLS)
General Technical Characteristics
Material Type: 2nd / 3rd generation single-crystal (SX) heat-resistant nickel-base superalloy.
Grade: CMSX-4 / CMSX-4 Plus (SLS).
Designation: CMSX-4, CMSX-4 Plus, CMSX-4 Plus SLS, Cannon-Muskegon SX-4.
Standards / Specifications: AMS (aerospace and power generation turbomachinery industry specifications), Rolls-Royce, Pratt & Whitney, GE, and Siemens Energy specifications.
Alloy Base: Nickel (Ni).
Alloying System: Ni-Co-Cr-Ta-W-Al-Re-Ti-Mo (Plus SLS version additionally features La/Y micro-alloying and ultra-low S).
Primary Manufacturing Method: Vacuum Induction Melting (VIM) followed by precision vacuum single-crystal investment casting.
Strengthening Mechanism: Precipitation hardening (approx. 68–72% $\gamma’$-phase) and solid-solution strengthening with rhenium, tungsten, and tantalum.
Key Properties: Ultimate creep-rupture strength (up to 1100–1150 °C), complete elimination of grain boundaries, and outstanding creep and thermal fatigue resistance.
Supply Forms: Ultra-high-purity cast remelt ingots (master alloy), single-crystal castings, and blanks.
Chemical Composition
| Element | CMSX-4, % | CMSX-4 Plus (SLS), % |
| Nickel (Ni) | Balance | Balance |
| Cobalt (Co) | 9.30 – 10.00 | 9.50 – 10.50 |
| Chromium (Cr) | 6.20 – 6.60 | 3.20 – 3.80 |
| Tantalum (Ta) | 6.30 – 6.70 | 7.70 – 8.30 |
| Tungsten (W) | 6.20 – 6.60 | 5.80 – 6.20 |
| Aluminum (Al) | 5.45 – 5.75 | 5.50 – 5.90 |
| Rhenium (Re) | 2.80 – 3.10 | 4.60 – 5.00 |
| Titanium (Ti) | 0.90 – 1.10 | 0.75 – 0.95 |
| Molybdenum (Mo) | 0.50 – 0.70 | 0.50 – 0.70 |
| Hafnium (Hf) | 0.07 – 0.12 | 0.07 – 0.12 |
| Carbon (C) | max 0.006 | max 0.006 |
| Sulfur (S) | max 0.001 (10 ppm) | max 0.0002 (less than 2 ppm) |
| Lanthanum + Yttrium (La+Y) | — | 0.005 – 0.020 (micro-additions) |
Mechanical and Performance Properties
ultra-high stress-rupture strength and creep resistance due to complete elimination of grain boundaries and the rhenium effect;
maximum resistance to thermal fatigue and thermal shock owing to the low elastic modulus of the single crystal in the
<001>orientation;exceptional adhesion of thermal barrier coatings (TBC) and platinum-aluminide coatings in the SLS modification (achieved by sulfur removal and lanthanum/yttrium gettering);
high phase stability without brittle topologically close-packed (TCP) phase precipitation over extended service life;
high creep-rupture ductility and resistance to fatigue crack propagation.
Density: approx. 8.70 g/cm³ (CMSX-4) / approx. 8.93 g/cm³ (CMSX-4 Plus SLS).
Melting Range: approx. 1320 – 1390 °C.
<001> crystallographic orientation accuracy and multi-stage heat treatment regimes, and are therefore governed by the documentation for a specific batch.Applications
single-crystal high-pressure turbine (HPT) rotor blades for modern commercial and military aircraft engines;
cooled first-stage turbine nozzle guide vanes and stator assemblies featuring intricate internal cooling passages;
high-temperature blades for ultra-high-efficiency industrial gas turbine units;
hot-section flowpath components for marine and aeroderivative gas turbine engines;
critically loaded elements in aerospace turbopump assemblies.
Key Features of CMSX-4 / CMSX-4 Plus (SLS)
rhenium alloying (3% in CMSX-4 and ~4.8% in CMSX-4 Plus), radically retarding diffusion-controlled creep;
SLS (Super Low Sulfur) technology in the Plus grade—reducing sulfur levels to under 1–2 ppm prevents protective oxide scale ($\text{Al}_2\text{O}_3$) spallation and multiplies thermal barrier coating life;
balanced tantalum alloying (up to 8%) to enhance $\gamma’$-phase strength and casting stability during solidification;
significant increase in turbine inlet gas temperatures, reducing specific fuel consumption and emissions;
ultra-high master alloy ingot purity, eliminating casting defects.